The Perkin Elmer Pyris 1 DSC Differential Scanning Calorimeter P/N N5370052 with Intracooler 2P Cooling Accessory Model FC100PEA1 and computer with preload Pyris Software features the fastest controlled heating and cooling rates and the fastest equilibration for isothermal analysis with calibration constancy. Excelling at the most difficult DSC analyses, the Pyris 1 DSC measures the amount of energy absorbed or released by a sample as it is heated, cooled, or held at a constant temperature.  

Specifications:
- Temperature Range: -170ºC to 730ºC
- Temperature Precision: ±0.1°C
- Dimensions (W x D x H): 40 x 63 x 51 cm
- Weight: 28 kg
- Electrical: 115V, 50/60Hz
 

The ALT Difference

  • Quality Used Lab Equipment
    All Items Tested to
    Manufacturer Spec
  • Used Microscopes For Sale
    More Than 12,000
    Items in Stock
  • Lab Equipment Warranty
    Up to 1-Year
    Warranty
  • Affordable Used Laboratory Equipment
    Price Match
    Guarantee
  • Discount Used Lab Equipment
    50%–80%
    off Retail

Join Our Mailing List

  • This field is for validation purposes and should be left unchanged.